Final report on SIM supplementary comparison 3.9: Type K thermocouple wire over the range 100 °C to 1100 °C

dc.contributor.authorDean C. Ripple
dc.contributor.authorK. M. Garrity
dc.contributor.authorM Araya
dc.contributor.authorCarlos R. Cabrera
dc.contributor.authorLiliana Murillo
dc.contributor.authorEulalia Vanegas
dc.contributor.authorDavid Gee
dc.contributor.authorElena Guillén
dc.contributor.authorSinuhé Martínez-Martínez
dc.contributor.authorE. Méndez-Lango
dc.coverage.spatialBolivia
dc.date.accessioned2026-03-22T15:55:49Z
dc.date.available2026-03-22T15:55:49Z
dc.date.issued2007
dc.descriptionCitaciones: 2
dc.description.abstractNRC publication: Yes
dc.identifier.doi10.1088/0026-1394/44/1a/03007
dc.identifier.urihttps://doi.org/10.1088/0026-1394/44/1a/03007
dc.identifier.urihttps://andeanlibrary.org/handle/123456789/55247
dc.language.isoen
dc.publisherIOP Publishing
dc.relation.ispartofMetrologia
dc.sourceNational Institute of Standards and Technology
dc.subjectThermocouple
dc.subjectMaterials science
dc.subjectRange (aeronautics)
dc.titleFinal report on SIM supplementary comparison 3.9: Type K thermocouple wire over the range 100 °C to 1100 °C
dc.typearticle

Files